Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® B3WG8 BK00564 - PA6-GF40 - BASF

Material Data Center offers the following functions for Ultramid® B3WG8 BK00564:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid B datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Product Texts
Glass fibre reinforced and heat aging resistant injection moulding grade, e.g.used for automobile parts with high stiffness requirements under the hood.
The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Processing/Physical Characteristicsdry / condUnitTest Standard
ISO Data
Melt volume-flow rate, MVR 20 / * cm³/10min ISO 1133
Temperature 275 / * °C -
Load 5 / * kg -
Molding shrinkage, parallel 0.3 / * % ISO 294-4, 2577
Molding shrinkage, normal 0.8 / * % ISO 294-4, 2577
Mechanical propertiesdry / condUnitTest Standard
ISO Data
Tensile Modulus 12700 / 7700 MPa ISO 527
Stress at break 205 / 125 MPa ISO 527
Strain at break 3 / 5.5 % ISO 527
Tensile creep modulus, 1000h * / 5400 MPa ISO 899-1
Charpy impact strength, +23°C 95 / 95 kJ/m² ISO 179/1eU
Charpy impact strength, -30°C 85 / 85 kJ/m² ISO 179/1eU
Charpy notched impact strength, +23°C 13 / 20 kJ/m² ISO 179/1eA
Charpy notched impact strength, -30°C 10 / 10 kJ/m² ISO 179/1eA
Thermal propertiesdry / condUnitTest Standard
ISO Data
Melting temperature, 10°C/min 220 / * °C ISO 11357-1/-3
Temp. of deflection under load, 1.80 MPa 210 / * °C ISO 75-1/-2
Temp. of deflection under load, 0.45 MPa 220 / * °C ISO 75-1/-2
Electrical propertiesdry / condUnitTest Standard
ISO Data
Electric strength 40 / 31 kV/mm IEC 60243-1
Other propertiesdry / condUnitTest Standard
Water absorption 5.45 / * % Sim. to ISO 62
Humidity absorption 1.8 / * % Sim. to ISO 62
Density 1460 / - kg/m³ ISO 1183
Diagrams
Viscosity-shear rate , Ultramid® B3WG8 BK00564, PA6-GF40, BASF
Shearstress-shear rate , Ultramid® B3WG8 BK00564, PA6-GF40, BASF
Dynamic Shear modulus-temperature , Ultramid® B3WG8 BK00564 (dry), PA6-GF40, BASF
Dynamic Shear modulus-temperature , Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Stress-strain , Ultramid® B3WG8 BK00564 (dry), PA6-GF40, BASF
Stress-strain , Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Secant modulus-strain , Ultramid® B3WG8 BK00564 (dry), PA6-GF40, BASF
Secant modulus-strain , Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Stress-strain (isochronous) 23°C, Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Creep modulus-time 23°C, Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Creep curve 23°C, Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Tensile modulus-temperature , Ultramid® B3WG8 BK00564 (dry), PA6-GF40, BASF
Tensile modulus-temperature , Ultramid® B3WG8 BK00564 (cond.), PA6-GF40, BASF
Characteristics
Processing
Injection Molding
Delivery form
Pellets, Black
Additives
Lubricants, Release agent
Special Characteristics
Heat stabilized or stable to heat
Applications
Automotive
Regional Availability
Other text information
Injection molding
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
injection molding, Dwell time, thermoplastics: 10 min
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.